Highlight 2

Atmospheric pressure chemical vapor deposition of α-Fe2O3 nanoparticles at 300 oC using 0.6 L min-1 N2 flow rate through the iron precursor bubbler presented an incorporated charge of 75 C cm-2 indicating reversibility after a period of 1400 s as obtained from chronoamperometry measurements.  Additionally, the charge transfer of Li+ across the α-Fe2O3 / electrolyte interface was enhanced presenting capacitance retention of 94 % after 500 scans.